High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Mo Cu Nb Al other no greater than 0Cr17Ni4Cu4Nb 0.07 1 1 0.035 0.03 15.5~17.5 3~5 - 3~5 0.15~0.45 - - 0Cr17Ni7Al 0.09 1 1 0.035 0.03 16~18 6.5~7.5 - ≤0.5 - 0.75~1.5 - 0Cr15Ni7Mo2Al 0.09 1 1 0.035 0.03 14~16 6.5~7.75 2~3 - - 0.75~1.5 - 0Cr15Ni5Cu4Nb 0.07 1 1 0.035 0.03 14~15.5 3.5~... -
17-4PH Material Data Sheet
International identifiers