Biphase Stainless Steel

  • SUPER DUPLEX S32760 / F55 / 1.4501

    Super Duplex S32760/ F55, Super Duplex Alloy UNS S32760 (F55 / 1.4501) xwedan berxwedanek hêja ye Pitting and Crevice Corrosion di ava deryayê de di germahiyên bilind de, ku bi PREN 40<(Berxwedana Pitting Eqv) ve tê peyda kirin. Di hawîrdorên tirş û klorîdê de li hember SCC (Qirkirina Korozyona Stresê) berxwedanek hêja.

  • SUPER DUPLEX 2507 Kalîteya Bilind

    ● UNS S32750, F53
    ● ASTM A 240, A790, A815, A182, A 276, A 476, A789
    ● EN 1.4410
    ● Navên din ên hevpar SAF 2507®

  • Biphase Stainless Steel

    Germahiya Bilind Pêkhatina kîmyayî Nota C Si Mn SP Cr Ni Mo Cu NW din ji F51 0.03 1 2 0.02 0.03 21~23 4.5~6.5 2.5~3.5 - 0.08~0.2 -0.2 -000 5 24-26 6 ~8 3~5 ≤0.5 0.24~0.32 — - F55 0.03 1 1 0.01 0.03 24~26 6~8 3~4 0.5~1 0.2~0.3 1 0.5 1 0.5 .035 23~28 3~6 1 ~3 - - - - A4 ...